Surface Analysis of Paper: Routledge Revivals

Autor Terrance E. Conners, Sujit Banerjee
en Limba Engleză Hardback – 7 mai 2019
First published in 1995, Surface Analysis of Paper examines surface analysis techniques from a paper industry perspective and places heavy emphasis on applications. Modern techniques, including ion mass spectrometry, infrared spectroscopy, and optical profilometry are reviewed in a straightforward manner. This new book provides details on widely used methods and instruments, and discusses how they can be used to attain, for example, contour maps of the microscopic constituents on paper surfaces and accurate analyses of the physical properties of paper.
Organized into three sections, Surface Analysis of Paper provides thorough coverage of the physical characteristics of paper, and a clear picture of new and emerging analytical methods. Carefully chosen background material on fundamental concepts is included wherever such material assists in understanding the uses of analysis methods.
Each chapter contains:
  • An introduction
  • A description of the technique
  • A discussion of the type of information that can be obtained with the particular technique
  • Practical examples to demonstrate the advantages of the technique
  • Citește tot Restrânge

    Din seria Routledge Revivals

    Preț: 149327 lei

    Preț vechi: 182107 lei
    -18%

    Puncte Express: 2240

    Carte tipărită la comandă

    Livrare economică 30 decembrie 26 - 13 ianuarie 27

    Livrare prin curier în România Termenul estimat este afișat lângă disponibilitate.
    Transport gratuit pentru acest produs Plată online sau ramburs, în funcție de opțiunile comenzii.
    Retur gratuit în 14 zile Comandă securizată și suport în română.

    Specificații

    ISBN-13: 9780367234690
    ISBN-10: 0367234696
    Pagini: 356
    Dimensiuni: 178 x 254 mm
    Greutate: 0.82 kg
    Ediția:1
    Editura: CRC Press
    Colecția CRC Press
    Seria Routledge Revivals


    Public țintă

    Professional

    Cuprins

    1. Physical Characterization of Surfaces.  2. Spectroscopic Methods.  3. Emerging Technologies.  Index.

    Recenzii

    "I certainly recommend Surface Analysis of Paper as a necessary volume for every reference library, and also for the personal library of any paper researcher who is also a materials scientist."
    -Journal of Pulp and Paper Science, Vol. 2, No. 5, May 1996

    Descriere

    First published in 1995, Surface Analysis of Paper examines surface analysis techniques from a paper industry perspective and places heavy emphasis on applications. Carefully chosen background material on fundamental concepts is included wherever such material assists in understanding the uses of analysis methods.