Nanoindentation of Natural Materials: Hierarchical and Functionally Graded Microstructures
Autor Arjun Dey, Anoop Kumar Mukhopadhyayen Limba Engleză Hardback – 24 sep 2018
It covers the basics of hierarchical and functionally graded structures and nanoindentation techniques and detailed discussion with correlation micro/nano mechanical-structures
The book includes practical issues backed with experimental data
Preț: 1072.87 lei
Preț vechi: 1601.12 lei
-33% Nou
Puncte Express: 1609
Preț estimativ în valută:
189.85€ • 222.62$ • 166.73£
189.85€ • 222.62$ • 166.73£
Carte tipărită la comandă
Livrare economică 31 ianuarie-14 februarie 26
Preluare comenzi: 021 569.72.76
Specificații
ISBN-13: 9781498784054
ISBN-10: 1498784054
Pagini: 238
Ilustrații: 10 Tables, black and white; 23 Illustrations, color; 106 Illustrations, black and white
Dimensiuni: 156 x 234 x 15 mm
Greutate: 0.43 kg
Ediția:1
Editura: CRC Press
Colecția CRC Press
ISBN-10: 1498784054
Pagini: 238
Ilustrații: 10 Tables, black and white; 23 Illustrations, color; 106 Illustrations, black and white
Dimensiuni: 156 x 234 x 15 mm
Greutate: 0.43 kg
Ediția:1
Editura: CRC Press
Colecția CRC Press
Public țintă
Professional Practice & DevelopmentCuprins
Chapter 1: Basics of hierarchical and functionally graded structures and mechanical characterization by nanoindentation—a paradigm shift for nano/micro-structural length scale
Chapter 2: Nanoindentation of bone: a tough hybrid composite
Chapter 3: Nanoindentation of teeth: a hard but tough hybrid functionally graded composite
Chapter 4: Fracture toughness of enamel region: role of DEJ and modeling of fracture toughness
Chapter 5: Nanoindentation creep of enamel and dentin tissues
Chapter 6: Nanoindentation of hair fiber: a tough hierarchical layered architecture
Chapter 7: Nanoindentation of shell and scale: a hard-tough layered functionally graded hybrid composite
Chapter 8: Combined nanoindentation and finite element approach in hierarchical and functionally graded structures
Chapter 9: Conclusions
Chapter 2: Nanoindentation of bone: a tough hybrid composite
Chapter 3: Nanoindentation of teeth: a hard but tough hybrid functionally graded composite
Chapter 4: Fracture toughness of enamel region: role of DEJ and modeling of fracture toughness
Chapter 5: Nanoindentation creep of enamel and dentin tissues
Chapter 6: Nanoindentation of hair fiber: a tough hierarchical layered architecture
Chapter 7: Nanoindentation of shell and scale: a hard-tough layered functionally graded hybrid composite
Chapter 8: Combined nanoindentation and finite element approach in hierarchical and functionally graded structures
Chapter 9: Conclusions
Descriere
The book will provide critical information regarding the basics of hierarchical and functionally graded structures and nanoindentation techniques along with detailed discussion with correlation micro/nano mechanical-structures. The readers will be able to identify the advantages of this method in purview of characterizing natural bio composites.