A Framework for Durability Design with Strain-Hardening Cement-Based Composites (SHCC)
Editat de Gideon P. A. G. van Zijl, Volker Slowiken Limba Engleză Hardback – 13 ian 2017
- Reflection on durability performance of existing applications in patch repair, a water reservoir and highway bridges.
- Guidelines for tensile testing towards durability assessment of cracked SHCC.
- New crack pattern related ingress rate indices for water and chloride into cracked SHCC. - The influence of low and high temperatures on SHCC durability performance.
- The mechanism of crack control reducing ASR and corrosion rate, and results on chloride-induced corrosion of embedded steel reinforcement.
- Self-healing of cracks in SHCC. - A conceptual durability design framework for SHCC and R/SHCC structures andmembers.
Preț: 695.84 lei
Preț vechi: 848.58 lei
-18%
Puncte Express: 1044
Preț estimativ în valută:
123.13€ • 146.81$ • 107.09£
123.13€ • 146.81$ • 107.09£
Carte disponibilă
Livrare economică 06-20 martie
Specificații
ISBN-13: 9789402410129
ISBN-10: 9402410120
Pagini: 220
Ilustrații: XX, 200 p. 123 illus.
Dimensiuni: 160 x 241 x 17 mm
Greutate: 0.54 kg
Ediția:1st ed. 2017
Editura: Springer
Locul publicării:Dordrecht, Netherlands
ISBN-10: 9402410120
Pagini: 220
Ilustrații: XX, 200 p. 123 illus.
Dimensiuni: 160 x 241 x 17 mm
Greutate: 0.54 kg
Ediția:1st ed. 2017
Editura: Springer
Locul publicării:Dordrecht, Netherlands
Cuprins
Preface.- Chapter 1 Introduction: Crack Distribution and Durability of SHCC, by Gideon van Zijl, Billy Boshoff, Christian Wagner and Volker Slowik.- Chapter 2 Transfer of Fluids, Gases and Ions in and Through Cracked and Uncracked Composites, by Christian Wagner, Volker Slowik, Gideon van Zijl, Billy Boshoff, Suvash Paul, Viktor Mechtcherine and Koichi Kobayashi.- Chapter 3 Fibre Durability, by Flavio Silva, Alva Peled, Bartosz Zukowski and Romildo Toledo Filho.- Chapter 4 Chemical Processes, by Erik Schlangen, Gideon van Zijl and Petr Kabele.- Chapter 5 Influence of Low Temperatures, by Koichi Kobayashi and Folker Wittmann.- Chapter 6 Influence of Elevated Temperatures, by Flavio Silva, Barzin Mobasher, Alva Peled, Dimas Rambo and Romildo Toledo Filho.- Chapter 7 Abrasion, by Volker Slowik, Steffen Müller, Christian Wagner and Viktor Mechtcherine.- Chapter 8 Behaviour of Bonded SHCC Overlay Systems, by Volker Slowik, Mladena Luković, Christian Wagner and Gideon van Zijl.- Chapter 9Reinforcing Bar Corrosion, by Koichi Kobayashi, Suvash Paul and Gideon van Zijl.- Chapter 10 Durability and Service Life Design Concepts for Structures and (Non-)Structural Members made of or Strengthened/Repaired with SHCC, by Viktor Mechtcherine, Frank Altmann and Gideon van Zijl.
Textul de pe ultima copertă
This book captures the state of the art of the durability of fibre-reinforced strain-hardening cement-based composites (SHCC) and the durability of structures or structural elements manufactured in full or in part with this class of modern construction materials. Highlights include:
- Reflection on durability performance of existing applications in patch repair, a water reservoir and highway bridges.
- Guidelines for tensile testing towards durability assessment of cracked SHCC.
- New crack pattern related ingress rate indices for water and chloride into cracked SHCC. - The influence of low and high temperatures on SHCC durability performance.
- The mechanism of crack control reducing ASR and corrosion rate, and results on chloride-induced corrosion of embedded steel reinforcement.
- Self-healing of cracks in SHCC. - A conceptual durability design framework for SHCC and R/SHCC structures andmembers.
- Reflection on durability performance of existing applications in patch repair, a water reservoir and highway bridges.
- Guidelines for tensile testing towards durability assessment of cracked SHCC.
- New crack pattern related ingress rate indices for water and chloride into cracked SHCC. - The influence of low and high temperatures on SHCC durability performance.
- The mechanism of crack control reducing ASR and corrosion rate, and results on chloride-induced corrosion of embedded steel reinforcement.
- Self-healing of cracks in SHCC. - A conceptual durability design framework for SHCC and R/SHCC structures andmembers.
Caracteristici
Provides a unique summary of the behaviour of a modern, high performance construction material Includes a special chapter proposing durability design guidelines Reports on the durability performance of recent applications Includes supplementary material: sn.pub/extras